22 Degree Angle Cut Ellipse
SP-3, F-33, H-33

22-Degree Angle Cut Ellipse Fortune Preformed Ceramic MediaFORTUNE ELLIPTICAL SHAPED MEDIA combines the finishing action of a flat shape with the flowing action of a cylindrical shape. Especially effective on concave surfaces. The elliptical shape has anit-wedging characteristics that reduce or eliminate lodging problems.

. SP-3 F-33 H-33 Size in
inches
ABC
Size in
millimeters
ABC
1 x 7/16 x 1 26 x 11 x 26
3/4 x 3/8 x 1 19 x 9.5 x 26
9/16 x 1/4 x 7/8 14.3 x 6.4 x 22.2
7/16 x 3/16 x 5/8 11 x 4.8 x 16
5/16 x 3/16 x 1/2 7.9 x 4.8 x 12.7

 